有些背面是石膏板???
楼主舒心点。。。
我之前porter davis造的房厕所地砖有几块都没平。。。走上去有个角凸起。。。最后折腾了半天也没返工。。。无解。。。
评论
那是做的差了点意思。。。。我建议product review那种网站写下差评如果大的builder的话。。。
小builder无解
评论
我最近一個五平米房間要舖瓷磚
四個邊跟中間差個一公分
師傅說要找平完再舖
就是先用水泥的leveller找平
乾了之後然後再舖瓷磚
另一個師傅說
不用先找平
舖的時候,低的地方放多點膠就好
我想舖不好就有你的問題產生了
所以我也好怕阿
晚點再去bunnings問意見
评论
先找平再铺是标准做法
评论
Tiling and the AS codes
The Australian Standard AS 3958.1:2007 is the criteria to the installation of a product or material in the tilelaying trade.
For example the adhesive coverage on a wall tile should align to the AS 3958.1:2007 as it recommends on p,84 for internal tiling to have 65% coverage and on external wall tiling to have 90% adhesive coverage respectively. On floor tiles the adhesive coverage should be 90%-100% for internal and external tiling there should be no voids around the edges of the floor tiles.
------------摘自http://www.tilespec.com.au/Tiling%20and%20the%20AS%20codes.html
希望信息正确
评论
地砖不能空,不管哪里,墙砖无所谓,十年经验瓷砖工在此
·找平做个tile bed 再做当然好,不过有时做了tile bed嫌地面太高会直接用glue点,做得好不会空,只是要用好胶 求分分
评论
謝謝你
评论
請問tile bed就是在水泥板上用水泥releveller?
用glue點的意思就是不做tile bed然後就是直接舖磚的時候glue放多一點就是?
第一個師傅說這樣做的話,瓷磚還是會往下沈。所以沒用
第二個師傅說,膠拌乾一點就好
請問您建議哪個好
评论
可以直接点,不过glue要用好的,如里用太差的就会沉,还要看地板怎么样,如果太差就要做tile bed
如果是bathroom 因为要流水,所以基本都是要做tile bed的 这样洗澡后水会流到floor watse中
评论
地砖都不能空,叫他重做,你的是水泥地(板除外 比如 FC cemnet 板),用手敲下,有声音都不行 没什么90%,只要是空谷以后都有问题
评论
地砖不能空,墙砖的确都是空的。关于误差去查一下standard & tolerance,直接google, 上面有具体的标准。我看了一下,确实是2毫米。
评论
用第一师傅吧
评论
建筑等水太深
评论
5%,是不会有声音的,反正用手敲,有声音就要换
评论
我看著師傅用點膠的方式舖我浴室牆磚
開了個帖
大部分人都說沒關係
還是好擔心哦
评论
百度上找的号称是国标的-----参考一下了。。。。
评论
地砖不能空啊。找builder算账。不行就投诉到fairtrading
评论
投诉
澳洲中文论坛热点
- 悉尼部份城铁将封闭一年,华人区受影响!只能乘巴士(组图)
- 据《逐日电讯报》报导,从明年年中开始,因为从Bankstown和Sydenham的城铁将因Metro South West革新名目而
- 联邦政客们具有多少房产?
- 据本月早些时分报导,绿党副首领、参议员Mehreen Faruqi已获准在Port Macquarie联系其房产并建造三栋投资联